The vat is filled about 2/3 with water this is treated with PH balance, I can only make the pulp in the vat acid free, the finished paper can pick up acid in the drying process only professionals who do this in labs can produce true acid free paper. I add about 8 cups of pulp and always SEED, so my cards can be planted by the recipient The screen is fitted with the frame and the pulp is scooped onto the screen , it takes a few trys in the beginning to get the right coverage and thickness